Skip to content

Ultem™ 9085

Note

Ultem™ 9085 is classified as an experimental material for advanced users.

Info

While you are free to use any brand and type of material you wish on your AON3D machine, we can only provide support for AON3D-approved materials that we have tested and developed processes for in-house, all of which can be purchased from AON3D directly by contacting sales@aon3d.com.

General Process Settings

Setting Value
Extrusion Temperature 340-395ºC
Bed Temperature 175ºC
Chamber Temperatures 115ºC

Usage Notes

Build Surface Preparation

Ultem™ 9085 prints best on the High Temperature PEI build plate with the use of a brim or raft. Note that surface of the PEI plate should be periodically resurfaced using a mill, or with an orbital palm sander if no milling services are available. Please contact sales@aon3d.com if you currently have a PEI film surfaced aluminum build plate and would like to upgrade to a High Temperature PEI Build Plate surfaced aluminum build plate.

Material Pre-treatment

Ultem™ 9085 is extremely susceptible to moisture uptake. We recommend drying the filament overnight (minimum 6-8 hrs) at 120ºC before use, and to always store backed material in a sealed container with silica dessicant. Take care to check the spool material of your filament prior to baking your material. Some vendors use low temperature materials for spools which may melt or deform at bakeout temperature.

Please contact help@aon3d.com for any questions on this matter.

Support Material

Breakaway Ultem™ support material is available. Do not expose the support material to high heat for extended periods of time since it may degrade and become brittle. Drying of support materials can be done at 45ºC overnight before use.


Sample Slicer Profiles

Assumes 0.6mm nozzle installed.

Ultem™ 9085: Single Extruder

Ultem™ 9085 with support material: Dual Extruder